Email:star15@alloyssi.com

1 2 3

product

self-hardening furan resin

Advantage of our furan resin: 1) Lower viscosity that is convenient to measure and easy to mix with sand. And the sand mold is in good mobility. 2) Lower free formaldehyde content with less smell that improve workers'working condition, and reduce pollu

We're here to help:  Easy ways to get the answers you need.

  • self-hardening furan resin
FOLLOW US:
Main Features:
 Advantage of our furan resin:

1) Lower viscosity that is convenient to measure and easy to mix with sand. And the sand mold is in good mobility.
2) Lower free formaldehyde content with less smell that improve workers'working condition, and reduce pollution of environment.
3)High strength that can reduce the cost of using less resin while also can improve quality of casting.
4) Good mobility of sand mold that reduce the workload of clean sand.
5) The casting produced by furan resin is in precision size, sharpe edge and smooth amd clean surface.




Specifications

Brand

density(20℃)

g/m³

Viscosity(20℃)

mpa.s≤

Free formaldehyde

(%)

 

Nitrogen content(%)≤

Quality guarantee periodyear)

Recommend applications

YX-730N

1.15-1.25

45

0.5

8

1

Cast iron and nonferrous metals

YX-635N

1.12-1.20

35

0.3

7

1

iron casting

YX-540N

1.12-1.20

30

0.3

5.5

1

iron casting

YX-445N

1.12-1.18

30

0.3

5

1

iron casting

YX-550N

1.10-1.20

30

0.3

4.5

1

iron casting

YX-655N

1.10-1.20

25

0.3

4

1

iron casting

YX-660N

1.10-1.20

20

0.3

3.5

1

Nodular cast iron

YX-370

1.10-1.18

25

0.3

1

1

Cast steel and large cast iron

YX-980

1.10-1.18

20

0.3

0.5

1

Large cast steel and alloy steel




Use parameter:

1.Sand: resin: curing agent=100:2:1 (weight ratio), Actual use is slightly lower

2. The sand

First add the curing agent into the raw sand and mix for 30-60 seconds. Then add the resin and mix for 30-60 seconds

3. After sand mixing, please immediately shape or core to avoid resin failure

 

 Packaging and storage

Sealed in plastic drums of 1 ton net weight, stored in a cool and dry place to avoid heat and direct sunlight;Resin can not be directly mixed with curing agent and other acidic materials, otherwise it will cause violent reaction, causing accidents.



 